We are professional Hastelloy G-30 G30 Alloy G30 G-30 UNS N06030 2.4603 Forged Forging Rings Rolled Rings Forging Sleeves Bushes Bushing Pipes Piping tubes tubings barrels Casing Cases Shells cylinders hubs housings Parts Pieces Material Products from china
The following sections will provide a detailed description of HASTELLOY(r) G30(r) alloy.
Chemical Composition
The following table shows the chemical composition of HASTELLOY(r) G30(r) alloy.
Element | Content (%) |
---|---|
Nickel, Ni | 43 |
Chromium, Cr | 28.0-31.5 |
Iron, Fe | 13-17 |
Cobalt, Co | 5 |
Molybdenum, Mo | 4-6 |
Tungsten, W | 1.50 - 4 |
Manganese, Mn | 1.50 |
Copper, Cu | 1 - 2 .40 |
Silicon, Si | 0.8 |
Phosphorous, P | 0.040 |
Carbon, C | 0.030 |
Sulfur, S | 0.020 |
Physical Properties
The physical properties of HASTELLOY(r) G30(r) alloy are given in the following table.
Properties | Metric | Imperial |
---|---|---|
Density | 8.22 g/cm³ | 0.297 lb/in³ |
Melting point | 1371ºC | 2500ºF |
Mechanical Properties
The mechanical properties of HASTELLOY(r) G30(r) alloy are given in the following table.
Properties | Metric | Imperial |
---|---|---|
Tensile strength | 1096 MPa | 159000 psi |
Yield strength (@0.2%) | 1000 MPa | 145000 psi |
Modulus of elasticity (plate heat treated to 1177°C, rapid quenched) | 202 GPa | 29300 ksi |
Elongation at break (in 50.8 mm) | 12% | 12% |
Reduction of area | 57% | 57% |
Hardness, Brinell (converted from Rockwell C hardness) | 304 | 304 |
Hardness, Knoop (converted from Rockwell C hardness) | 326 | 326 |
Hardness, Rockwell C | 32 | 32 |
Hardness, Vickers (converted from Rockwell C hardness) | 316 | 316 |