Inconel 625 UNS N06625 2.4856 Alloy 625 NiCr22MO9Nb Forged Forging steel Rings Rolled Rings Forging Sleeves Bushes Bushing Pipes Piping tubes tubings barrels Casing Cases Shells cylinders hubs housing
型号:
parameters1:
parameters2:
parameters3:
parameters1:
parameters2:
parameters3:
We are professional Inconel 625 UNS N06625 2.4856 Alloy 625 NiCr22MO9Nb Forged Forging steel Rings Rolled Rings Forging Sleeves Bushes Bushing Pipes Piping tubes tubings barrels Casing Cases Shells cylinders hubs housings Parts Pieces Material Products from china
Chemical Composition
C | Si | Mn | P | S | Cr | Mo | Ni | Cu | Nb | Ti | Fe | Co | Al | Cb+Ta | ||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
2.4856 | Min % | 20,00 | 8,00 | 58,00 | 3,15 | |||||||||||
Max % | 0,10 | 0,50 | 0,50 | 0,02 | 0,015 | 23,00 | 10,00 | 0,50 | 4,15 | 0,40 | 5,00 | 1.00 | 0,40 | |||
(Key to Steel 2010) | ||||||||||||||||
alloy 625 N 06625 | Min % | 20,00 | 8,00 | 58,00 | 3,15 | |||||||||||
Max % | 0,10 | 0,50 | 0,50 | 0,015 | 0,015 | 23,00 | 10,00 | . | 0,40 | 5,00 | 0,40 | 4,15 | ||||
ASTM B704 |
Physical properties
Property | Value |
---|---|
Density: lb/in.3 | 0,303 |
Hardness: HB | <=240) |
Permeability at 20°C/68°F | 1,003 |
magnetizabe | paramagnetic |
Temperature T °C/F (°C/F) | Specific heat J / kgK (Btu / lb °F) | Thermal conductivity W/mK (Btu·in / ft2·h·°F) | Electric resistance µΩ · cm (Ω circ mill / ft) | Modulus of elasticity kN/mm2 (103 ksi) | Expansion rate from 70°F bis T 10-6 / K (10-6 / °F) |
---|---|---|---|---|---|
20 / 68 (93 / 200) | 415 (0,099) ((0,103) | 9,8 (68) (77) | 128 (770) (782) | 209 (30,3) (29,4) | (7,0) |
200 /392 (204 / 400) | 460 (0,110) | 12,8 (90) | 132 (794) | 195 (28,3) | 13,1 (7,7) |
400 / 752 (427 / 800) | 505 (0,122) | 16,3 (0,115) | 135 (815) | 185 (26,5) | 13,7 (7,6) |
600 /1112 (649 / 1200) | 550 (0,134) | 19,3 (139) | 136 (820) | 170 (24,1) | 14,6 (8,3) |
800 /1472 (871 / 1600) | 600 (0,147) | 22,6 (167) | 136 (815) | 153 (21,0) | 15,8 (9,0) |
1000 /1832 | 650 | 26,7 | 132 | 128 | 17,0 |
Mechanical properties (20°C / 68°F)
Density (lb/in.3) | 0,303 | ||
---|---|---|---|
Yield strength Rp0,2 (ksi) | 60-50 | ||
Tensile strength MPa bei RT | 820 -1050 | ||
Elongation A5 (68°F) (%) | >=30 | ||
Impact energy ISO-V (J/cm2) | >= 125 | ||
average at room temperature (J/cm2) |